Mechanical properties
VAUTID heat resistant cast iron is used for industrial furnace engineering (up to 1.150 °C), for stirring teeth (up to 1.100 °C) and for petroleum and natural gas plants (up to 1.100 °C).
VAUTID material | Tensile strenght [N/mm²] |
Yield strenght [N/mm²] |
Enlongation after fracture (Lo=5d) min. |
Hardness HB (HRC) |
VAUTID H – 1.47291 | – | – | – | max. 300 |
VAUTID H – 1.47432 | – | – | – | d |
VAUTID H – 1.47762 | – | – | – | d |
VAUTID H – 1.47772 | – | – | – | d |
VAUTID H – 1.48232 | min. 550 | min. 250 | 3 | d |
VAUTID H – 1.48252 | min. 450 | min. 230 | 15 | – |
VAUTID H – 1.48262 | min. 450 | min. 230 | 8 | – |
VAUTID H – 1.48372 | min. 450 | min. 220 | 6 | – |
VAUTID H – 1.48482 | min. 450 | min. 220 | 8 | – |
Condition of delivery: 1 WB; 2 G